Material: | Aramide Yarn |
---|---|
Feature: | Abrasion-Resistant, Anti-Distortion, Heat-Resistant |
Fiber Type: | Filament |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Typical Technical Properties:
1) After 1500 Sunshine hours, its remaining strength is more than 80%.
2) After 6 months in most chemicals (seawater, gas, etc), its remaining strength is 100%.
3) The UHMWPE ropes remaining strength is 100% after 1000 times loaded rotative test.
4) Its rotative times until break of Abrasion proof are more than 110 by 103.
5) Its rotative times until break of Winding proof are more than 240 by 103.
6) Its strength of annelation is 12 up to 18g/d. its 10 up to 15g/d for collusion.
7) Melting Point is around 135 145
Over 10 times stronger than steel, 40% greater than aramid fiber, good resistant to UV and typical using for high performance fishing line. Feature:
- Low density
- High strength
- High energy absorption
- Low dielectric constant
- High electromagnetic wave transmission
- Low friction,
- Impact resistance
Application:
National defense
Public security
Naval vessels
Aviation
Ocean oil
Medical treatment, gymnasium, etc
Specification Sheet:
Name | Breaking Tenacity(CN/dtex) | Initial Modulus(CN/dtex)(Average) | |
Excellent | Qulified | ||
XT-30 | ≥34 | ≥32 | ≥1200 |
XT-40 | ≥34 | ≥33 | ≥1200 |
XT-50 | ≥34 | ≥32 | ≥1100 |
XT-60 | ≥34 | ≥32 | ≥1100 |
XT-75 | ≥34 | ≥32 | ≥1100 |
XT-100 | ≥34 | ≥32 | ≥1100 |
XT-125 | ≥32 | ≥30 | ≥1000 |
XT-150 | ≥32 | ≥30 | ≥1000 |
XT-175 | ≥32 | ≥30 | ≥1000 |
XT-200 | ≥32 | ≥30 | ≥1000 |
XT-250 | ≥32 | ≥30 | ≥1000 |
XT-300 | ≥30 | ≥28 | ≥900 |
XT-350 | ≥30 | ≥28 | ≥900 |
XT-400 | ≥30 | ≥28 | ≥900 |
XT-500 | ≥30 | ≥28 | ≥900 |
XT-600 | ≥30 | ≥28 | ≥900 |
XT-700 | ≥30 | ≥28 | ≥900 |
XT-800 | ≥28 | ≥26 | ≥800 |
XT-1000 | ≥28 | ≥26 | ≥800 |
XT-1200 | ≥28 | ≥26 | ≥800 |
XT-1600 | ≥28 | ≥26 | ≥800 |